Epoxy Dome Stickers is a printed label consisting of a two-part epoxy resin coating. The resin unfurled on its own, forming a raised lens-like lid. The core of the cap is usually 0.8-2.5 mm thick and the printed edges are getting thinner.
The process starts with printing artwork on the substrate. The surface is then treated so that the resin can attach to the surface. Add a certain amount of mixed resin with a needle or positive displacement valve. Surface tension then pulls the resin into a dome. Resin solidifies for minutes to hours.
There was no mold in the dome. This process can be used to create a badge or 50,000 badges.

"Dome" Is a Geometry, Not a Decoration

The dome label defines meniscus, not just coating. Resin is used as a narrow bead to add about the same width to an artwork outline. Surface tension pulls the resin outward and upward until it stops at the edge of the printing area. The result is a ball cap. It had a thick center and thin edges. It also has a curved surface like a weak lens. This curve creates optical depth that makes the figure look like it's under glass. It also makes the print look a little larger. Because of this, fine text below 4pt and lines under 0.1mm look soft inside the dome.


The shape comes from the surface properties of the material, not from the mold. So, there are three main factors that determine whether the dome looks like glass or a puddle::

Resin viscosity-If the resin is too thin, it spreads to the edges of the artwork and loses its shape. If it's too thick, it doesn't level well and can leave a raised blob with tool marks.

Base Surface Energy-The resin must moisten the surface around the printing area well enough to keep it on the edge. If the surface is dirty or untreated, the resin can be pulled back. This can create uneven or uneven edges.

Dispensed volume per unit area-this controls the thickness of the dome. There is no molds to stop the resin flow.

The Chemistry Behind the Cap

Two-component epoxy doming resin is made from bisphenol bisphenol A diglycidyl ether and a curing agent. Cyclolipids are often used outdoors. An aliphatic amine is usually used to solidify quickly at room temperature. If curing is possible at higher temperatures, acetic anhydride is used.
The two components are supplied in a fixed proportion. Common ratios are 1:1 or 2: 1 volumetric. Proportionality has to be accurate. The ratio should be within about ±2 percent of the correct ratio. This helps create a hard, dry, clear hat. If the ratio is not right, the surface may become slightly sticky or waxy.

Resin system

Mix ratio (typical)

Working life at 25 °C

Shore hardness after full cure

UV behaviour

Where it fits

Fast aliphatic amine epoxy

1:1 by volume

15–30 min

80–85 D

Yellows noticeably in direct sun

Indoor badges, promotional items

Cycloaliphatic amine epoxy

2:1 by volume

30–60 min

82–86 D

Good with UV package

Outdoor nameplates, equipment labels

Anhydride-cured epoxy

1:1 or 100:80 by weight

60–120 min, needs heat cure

85–88 D

Best transparency retention

High-clarity lens work

Two-part polyurethane

1:1 by volume

20–40 min

65–80 A

Very low yellowing

Flexible films, curved surfaces

UV-cure acrylic

Single component

Unlimited until exposed

75–85 D

Moderate

High-throughput flat work

The most important option is epoxy or polyurethane. Epoxy is harder, smoother and more abrasive. It can handle keys, coins, and regular industrial wiping. Polyurethane is more flexible and stays clean outdoors for longer. As a result, it is commonly used in thin vinyl labels and products that require bending. An outdoor label that cracks along the curved surface a few years later might have an epoxy cap, and polyurethane would be a better choice.
Two other features also affect the process. Viscosity of doming resin at casting temperature is usually 2,000 -6,000 mPa s. This is low enough for the resin level itself in a matter of seconds. It is also high enough to hold a 2mm dome without a dam.
Working life is the amount of time available before the resin mixture becomes too thick to distribute well. Usually around 15–60 minutes. The timing depends on the solidifying agent and room temperature. Mixed resin also produces heat as it solidifies. The large amount of gel left in the mixing cup can be faster than the same resin when it is distributed immediately.

The Manufacturing Sequence, Step by Step

Printing. Artwork is printed on the substrate. Common substrates include cast ethylene, polyester, polycarbonate, anode aluminum, powder coating metals, and pressure-sensitive label stocks. Screen printing is still common because it produces a thick layer of ink. This layer will remain clear and strong under the dome. It also helps form the edges of the fixed resin.

Substrate preparation. The substrate is cut into the desired shape. Its surface has also been treated to increase surface energy. Corona or plasma treatment of about 38 dyn/cm or more is a common method for low-surface-energy plastics. Metal and glass usually require primer. If you skip this step, the resin may form a good sample during testing, but the edges may be raised after use.

Fixture loading. Parts are placed on trays or registration pins. This causes the dispensing head to follow the same path for each segment. Positioning tolerances were generally ±0.3 mm. The fixture maintains this accuracy throughout the run.

Measurement and mixing. Resins and curing agents are pumped through a metering system. Gear pump is used to improve accuracy. Pressure-time system is simpler. The two materials are then mixed in a static mixer or an inline dynamic mixer. The mixing ratio is checked against the supplier's data sheet. Since the pump's accuracy varies with wear and tear, samples can also be assigned to the scale to check proportions.
V. Busch. Mixed resin is added as a bead or patterned back and forth inside the edges of the artwork. Stitches are selected based on the resin viscosity and flow of the resin. The amount of resin controls the thickness of the dome.
For caps with h height and a radius, the volume is:
Indry-adhesive labels with a diameter of 25 mm and a central height of 1.5 mm, with a volume of about 0.37 mL each. Multiply by the number of parts on the paper to estimate the total amount of resin needed for the job.

Outflow. Resin diffuses and levels itself in 20 to 40 seconds. In the meantime, keep air off the ground. Do not touch or shake the tray. Movement can cause the dome to be uneven and may not be able to return to its original shape.

degassing. Air produced during mixing process rises as bubbles. Low-viscosity resin can release these bubbles on its own in a minute or two. Thicker resin and fast-curing hardeners may require vacuum degassing before dispensing. Another option is to pass through the tray via the heating channel. Heating reduces the viscosity of the resin in the short term and helps the bubbles escape.

cures. At room temperature, it usually takes 2–8 hours resin to harden enough. Full hardness usually develops after 24 hours or more. Curing at 50-60 °C can shorten the curing time to about 30–60 minutes. However, this increases the risk of the amine-cured systems turning yellow. It also hardens the resin faster in mixing containers.

(iii) Examination of transformation. Check the finished product for several problems. These include domes that don't stop at the edge of the print, bubbles larger than the permitted size, and uneven thickness throughout the paper. Then flatten the parts. Do not stack the domes under pressure until fully cured. Partially cured resin can form a permanent flat spot.

Why the Dome Holds Its Shape Without a Mould

The same basic physics applies to 15 mm markings and 200 mm control panel surfaces. The resin spreads outward until it reaches the edge of the ink. The surface energy changes at this point, so the resin stops at the edge. Then the liquid was like a controlled droplet. Gravity flattens large domes, while surface tension keeps small domes round. For a typical 2,000–4,000 mPa·s resin, this change usually occurs in domes 40 – 60 mm in diameter. After that, gravity is more powerful. The center becomes flatter, so the cap looks more like a thin coating than a lens.
This leads to three practical outcomes. First, very large domes are usually divided into smaller print areas. They can also use raised dams. This can be a place to print or add borders of about 0.3–0.6 mm high to keep resin in place.
Secondly, the addition of thixotropy, such as fumed silica, helps the resin retain a higher shape. But it reduces gloss slightly and captures more air.
Third, the resin that makes the smooth 20mm dome can form an orange peel surface on a 150mm panel. Resins must travel further on larger panels. This gives the surface more time to form a skin before the resin finishes the level.

Adhesion: Where Domed Labels Fail First

resin cap are usually the last part to fail. The bond between the print, substrate and adhesive usually determines the label's service life.

  • Over time Plasticised vinyl releases plasticizers. The plasticiser can be moved into resins and adhesives. This softens the edges of the dome and causes it to rise. A heavier dome would make it worse because it would add more tension to the edges.
  • Polycarbonate cracks when it comes into contact with solvents. Inks and primers that work well on vinyl can cause small cracks in polycarbonate when the panels are subjected to stress from solidifying domes.
  • Polypropylene and polyethylene have a surface capacity of less than 31 dyn/cm. Without corona or flame treatment, adhesion is unreliable even if the resin flows well.
  • Powder-coated metals can adhesion results very differently. The coating type, curing degree and age of powder batch will affect its adhesion. Therefore, it is necessary to test the actual coated panels.
  • Flexible or curved substrates require a flexible dome. Hard epoxy domes also cracks when the substrate bends slightly. This is why polyurethane is often used in curved surfaces.

Yellowing, Weathering, and Light Stability

Clarity retention should be measured, not assumed. Two main measurements were used: yellowness index and colour difference, such as ΔE compared to an unexposed sample. Both were tested during accelerated weathering. A xenon-arc or fluorescent UV test system are typically used for about 500–1,000 hours. Gloss can also be measured during testing.
Aromatic amine hardeners is a common cause of early yellowing. Cyclic lipids with a UV absorber and a hindered-amine light stabiliser help keep the dome clean for longer. cure temperature is also important. It's important to Keeping it at the low end of the vendor recommendation range. Too much heat during curing can cause discoloration, similar to prolonged exposure to sunlight.
Gloss is another useful sign. A dome can maintain a good yellowness index but lose several glossy units. This can mean the surface has started to chalk or develop very small cracks. Then the surface may fail.

Failure Modes and Their Causes

Symptom

Mechanism

Corrective action

Fisheyes, craters, edge pull-back

Surface contamination or low surface energy

Clean with a compatible solvent, corona or plasma treat, add flow agent

Bubbles above spec size

Air entrained during mixing, or solvent outgassing from ink

Vacuum degas batch, mix slower and lower, flash off ink before doming

Orange peel texture

Viscosity too high or substrate too cold

Warm resin and substrate to 22–25 °C, adjust formulation

Tacky, never fully hard surface

Off-ratio metering or amine bloom from humidity

Recalibrate pumps, verify by weight, control room humidity

Edge lift after weeks in service

Adhesion failure, plasticiser migration, or peel load from an oversized dome

Primer, substrate change, reduce dome mass, softer resin

Cracks or crazes radiating from the print

Solvent attack on stressed plastic, or thermal shock

Substrate-compatible inks, reduce exotherm, gradual cooling

Dome flattens in the centre

Gravity on an oversized dome, or too low a viscosity

Print a dam, raise thixotropy, split the field

Yellowing in service

Aromatic hardener plus UV exposure, or overheat cure

Cycloaliphatic system with UV package, lower cure temperature

Quality Checks That Predict Field Performance

A doming line that controls six key points is unlikely to produce a batch of poor-quality Epoxy Dome Stickers. First, check the ratio by weight. The the resin viscosity is then checked against the specification. Confirm gel time with fresh sample. Cure adhesion was tested by transectional or tensioning tests. Measure the thickness of the center and edges of the dome. Compare the appearance of the finished product with a retained approved sample.
For outdoor or industrial use, accelerated weathering, yellowness and abrasion resistance also tested. If the dome label contains safety, warning or equipment identification information, the durability standards of the relevant label also applies. For products made for children, the chemical and physical requirements the finished product take precedence over label-level testing.

When a Dome Is the Wrong Answer

Domed labels aren't always the best option. They may not be suitable for substrates that release gases over time, films that bend sharply, surfaces of untreated polyolefin surfaces, or parts that remain above 100 °C. When labels need to be washed completely from the surface, they don't fit either. The 1.5mm raised lid can be secured to a squeegee, conveyor guide or moulded groove.
For orders of less than a few hundred items, hand-dispensed doming is usually the cheapest option. The unit cost of ordering tens of thousands of identical flat pieces, molded or cast plastic pieces may be lower.
Epoxy doming are usually used for small and medium-sized production runs with different artworks. It's also useful when labels need good scuff resistance and a quality look without the cost of a tool.

 

Frequently Asked Questions

How thick should the dome be?
The dome is 0.8 – 1.5 mm in height and a 15–30 mm part, putting it in the practical range. It provides enough curves to create a lens effect, but keeps the load low on the edges. Larger panels are typically 1.5 – 2.5 mm. Over 3mm, the dome gets heavier and the curing time gets longer. It is also more likely to crack at the edges when the part bends or undergoes temperature changes.
Can domed labels be applied to curved or flexible surfaces?
Yes. ' Use a flexible polyurethane cap instead of a hard epoxy cap. Adhesives should also match the surface energy of the target material. Hard covers with a radius of less than 25mm can crack over time, even if they look fine in application.
How long do they last outdoors?
A well-designed lid usually provides good clarity and adhesion for three to five years in temperate conditions. A cycloaliphatic hardener, UV absorber and light stabiliser can help. The cure temperature should be near the low end of the recommended range. In practical applications, imprints and adhesives tend to limit service life before resins. Accelerated weathering tests are useful for comparing different systems, but they do not guarantee a specific service life.
Do they need a special printer or ink?
No special printing process is required. But ink cannot contain solvents, attack substrate or blend resin. Printing areas must also be completely dry before dispensing. Many doming problems seem to stem from the resin actually starting to dry out with solvents left in the ink layer.

Conclusion

The attraction of Epoxy Dome Stickers comes from the process of forming the resin itself. Mix the two ingredients in the correct proportions. A certain amount of control is sprinkled on properly treated prints. The surface tension then forms a dome.
The process is simple, but the details matter. The ratio was controlled to ± ±2 percent. Keep surface energy above 38 dyn/cm. Keep the dome below 2.5mm. Use a treatment schedule that avoids temperatures that reduce clarity. Match the resin to the softness of the substrate.
These five things help label handle long-term use, weather, keys and industrial cleanliness. If left unchecked, even the dome's high-gloss surface raises the edges.

Sources

ISO 1519, Paints and varnishes - Bend test (cylindrical mandrel)

ISO 2409, Paints and varnishes - Cross-cut test

ISO 2811-1, Paints and varnishes - Determination of density, Part 1: Pycnometer method

ISO 3219-1, Rheology - Vocabulary and symbols for rotational and oscillatory rheometry

ISO 9514, Paints and varnishes - Determination of the pot life of multicomponent coating systems

ISO 11357-1, Plastics - Differential scanning calorimetry (DSC), Part 1: General principles

ISO 4892-2, Plastics - Methods of exposure to laboratory light sources, Part 2: Xenon-arc lamps

ISO 6272-1, Paints and varnishes - Rapid-deformation (impact resistance) tests, Part 1: Falling-weight test, large-area indenter

ASTM D523, Standard Test Method for Specular Gloss

ASTM D2244, Standard Practice for Calculation of Color Tolerances and Color Differences from Instrumentally Measured Color Coordinates

ASTM E313, Standard Practice for Calculating Yellowness and Whiteness Indices from Instrumentally Measured Color Coordinates

ASTM D3359, Standard Test Methods for Rating Adhesion by Tape Test

ASTM D4060, Standard Test Method for Abrasion Resistance of Organic Coatings by the Taber Abraser

ASTM D2471, Standard Test Method for Gel Time and Peak Exothermic Temperature of Reacting Thermosetting Resins

ASTM G154, Standard Practice for Operating Fluorescent Ultraviolet (UV) Lamp Apparatus for Exposure of Nonmetallic Materials

UL 969, Standard for Marking and Labeling Systems

ISO 9001, Quality management systems - Requirements

Send Inquiry