Waterproof Electroplating Nickel Logo


How to make nickel sheet Waterproof Electroplating Nickel Logo?
Waterproof Electroplating Nickel Logo processing and manufacturing process
Photosensitive and development
- Photosensitive:
- Firstly check whether there are eyelets and scratches on the film. Eyelets with a diameter of less than 0.5MM and scratches with a diameter of less than 0.2MM can be repaired with a black pen. Excessive eyelets and scratches can be directly discarded.
- Next, check whether there are black spots and dust on the glass of the exposure machine, and clean it if there is any.
- Then take the film sheet and attach it to the stainless steel. Be careful not to paste it backwards when attaching it. The side of the film sheet should face down and place it on the glass.
- Turn on the lamp at the end, vacuuming time is 25±5 seconds, exposure time is 28±3 seconds: the exposure is completed and transported to the development workshop through the transmission output port.
- Development:
- The operator dips the exposed stainless steel plate into the developer solution, and puts 4-6 pieces each time.
- The soaking time should not exceed 1 minute. If the time is too long, the ink will fall off easily.
- Gently wipe the developing surface with a sponge until it is fully formed.
- Rinse the surface with clean water, and visually inspect the surface for miscellaneous spots, scratches and missing stars. If the development is not sufficient, it needs to be reworked, and other poor development is directly discarded.
Application

Production Process

Our Sample Room










Hot Tags: waterproof electroplating nickel logo, China, suppliers, manufacturers, factory, customized, wholesale